Your Position: Home > Technical Data > Metal Materials
    Grades of Metal Materials



    Forged Cast Forged Cast
    ASTM A105
    A182 F316
    A182 F316L
    2.4816/ N06600
    A216 WCB
    A351CF8M
    A361CF3M
    Inconel600 
    A182 F11
    A182 F304
    A182 F304L
    ASTM A104
    A217 WC6
    A351CF8
    A351CF3
    WCC
    Physical Properties of Metal Materials

    Temperature Resistance

     
     
    Temperature range
     
    Working conditions
    Material selection
    Remarks
    Ultra-low temperature
    -254 (liquid hydrogen)~-101℃ (ethylene
    LNG, air separation Austenitic stainless steels ASTM A351 CF8M, CF3M, CF8 and CF3, ASTM A182 F316, F316L, F304 and F304L, ASTM A433 316, 316L, 304, 304L and CF8D The body material must be austenitic stainless steel with a face-centered cubic lattice, copper alloy or aluminum alloy, and its low-temperature mechanical properties after heat treatment, especially the low-temperature impact toughness, must meet the requirements of the standard. Must deep cryogenic treatment be carried out in liquid nitrogen (-196℃)?
    Low temperature
    -100~-30℃
    Low-temperature methanol washing Low-temperature austenitic stainless steels include ASTM A351 CF8M, CF3M, CF8 and CF3, ASTM A182 F316, F316L, F304 and F304L, ASTM A433 316, 316L, 304, 304L and CF8D. Ferritic and martensitic steels for low-temperature pressure-bearing parts include ASTM A352 LCA(-32℃), LCB, LCC(-46℃), LC1(-59℃), LC2, LC211(-73℃) and LC3(-100℃)
    The initial price of the materials in the ASTM A352 standard is relatively low, but their chemical composition during melting must comply with reliable and very strict in-plant control standards. Their heat treatment process is complicated and requires repeated quenching and tempering before the low-temperature impact toughness required by the standard can be achieved, and the production cycle is long. When the low-temperature impact toughness does not meet the requirements of the standard, the material is not allowed to be put into production as low-temperature steel. Therefore, they are only used when the production batch is large and furnace melting is possible; under normal circumstances austenitic stainless steel is selected.
    Sub-high temperature
    325~425℃
    Power plant steam, superheated water, atmospheric and vacuum distillation units and delayed coking units of refineries For water and steam, WCB, WCC, A105, WC6 and WC9 are mainly used. When the medium is sulfur-containing oil, C5, CF8, CF3, CF8M and CF3M etc., which resist sulfide corrosion, are mainly used. They are mostly used in the above applications; at this time the valves of CF8, CF8M, CF3 and CF3M materials are not used to resist acid solution corrosion, but for sulfur-containing oil and oil-gas pipelines. In this working condition, the upper limit of the maximum working temperature of CF8, CF8M, CF3 and CF3M is 450℃
    Carbon steel for valves refers to WCB and WCC cast steel in the ASTM A216 standard and ASTM A105 forged steel. The suitable working temperature of carbon steel for valves is -29~425℃. However, for safety, considering that the working temperature of the medium may fluctuate, the service temperature of ordinary carbon steel should generally not exceed 400℃.
    High-temperature Class I
    425~550℃
    Power plant superheated steam If the working medium is water or steam, although the high-temperature steels WC6 (t≤540℃) or WC9 (t≤570℃) can also be used, and in the case of sulfur-containing oil, although the high-temperature steel C5 (ZG1Cr5Mo) can also be used The body material of Class PI valves is the “high-temperature Class I medium-carbon chromium-nickel rare-earth titanium high-quality heat-resistant steel” based on CF8 in the ASTM?? A351 standard
    High-temperature Class II
    550~650℃
    Heavy oil catalytic cracking unit The body material of Class PII valves is the “high-temperature Class II medium-carbon chromium-nickel rare-earth titanium tantalum-strengthened heat-resistant steel” based on CF8 in the ASTM A351 standard  
    High-temperature Class III
    650~730℃
    Heavy oil catalytic cracking unit The “high-temperature Class III medium-carbon chromium-nickel-molybdenum rare-earth titanium tantalum-strengthened heat-resistant steel” based on CF8M in the A351 standard  
    High-temperature Class IV
    730~816℃
      The body material of Class PIV valves is the “high-temperature Class IV medium-carbon chromium-nickel-molybdenum rare-earth titanium tantalum-strengthened heat-resistant steel” based on CF8M in the ASTM A351 standard. CK-20 and F310 (with C content ≥0.050%) and F310H etc. heat-resistant stainless steels in the ASTM A182 standard  
    High-temperature Class V
    >816℃
    Flue HK-30 and HK-40 superalloys in the ASTM A297 standard  
    Hardness Hardness indicates the ability of a material to resist the indentation of a hard object into its surface. It is one of the important performance indicators of metal materials. Generally, the higher the hardness, the better the wear resistance. The commonly used hardness indicators are Brinell hardness, Rockwell hardness and Vickers hardness.
    1. Brinell hardness (H
    With a certain load (generally 3000kg), a hardened steel ball of a certain size (generally 10mm in diameter) is pressed into the surface of the material; after holding for a period of time and removing the load, the ratio of the load to the area of the indentation is the Brinell hardness value (HB), in units of kilogram-force/mm2 (N/mm2).
    2. Rockwell hardness (HR)
    When HB>450 or the specimen is too small, Brinell hardness cannot be used and Rockwell hardness is used for measurement instead. A diamond cone with an apex angle of 120° or a steel ball with a diameter of 1.59 or 3.18mm is pressed into the surface of the material under test under a certain load, and the hardness of the material is obtained from the depth of the indentation.
    According to the different hardness of the test material, three different scales are used to express it:

    HRA: the hardness obtained by using a 60kg load and a diamond cone indenter, used for materials of extremely high hardness (such as cemented carbide, etc.).
       HRB: the hardness obtained by using a 100kg load and a hardened steel ball of 1.58mm diameter, used for materials of relatively low hardness (such as annealed steel, cast iron, etc.).  
       HRC: the hardness obtained by using a 150kg load and a diamond cone indenter, used for materials of very high hardness (such as hardened steel, etc.). 
    Steliete hardness 45 HRC, Chromium Carbride hardness 70HRC, Tungsten Carbride hardness 85HRC

      3. Vickers hardness (HV)

        With a load of up to 120kg and a diamond square pyramid indenter with an apex angle of 136° pressed into the surface of the material, the surface area of the indentation pit is divided by the load value, which is the Vickers hardness HV value (kgf/mm2).

     Hardening methods:
    1. Heat treatment, such as surface precipitation hardening heat treatment; the main materials are 440/630;
    2. Surfacing with Stellite alloy
    3. Plating superhard alloys by chemical means, such as hard chromium plating, tungsten carbide, nickel-based alloys, etc.; there are also means such as low-temperature nitriding treatment, ceramic spraying, etc.
    Low-carbon stainless steels such as 304L and 316L are not suitable for Stellite hardfacing.
    According to the German standard DIN50150, the following is a comparison table of the tensile strength of steel versus Vickers hardness, Brinell hardness and Rockwell hardness in the commonly used range.
    1. Shore hardness (HS) = Brinell hardness (BHN)/10+12  2. Shore hardness (HS) = Rockwell hardness (HRC)+15  3. Brinell hardness (BHN) = Rockwell hardness (HV)  4. Rockwell hardness (HRC) = Brinell hardness (BHN)/10-3

    High-hardness treatment methods:
    Plasma spraying (APS): the APS process uses a high-voltage arc to heat a gas stream, thereby producing a high-velocity plasma jet. The plasma generating gas is usually argon containing a small amount of hydrogen or helium, so that the fed powder is effectively heated and melted. The temperature of the plasma arc core is usually above 10000K, and the particle impact velocity can be as high as 250m/s
    High-velocity oxy-fuel spraying (HVOF): in the HVOF spraying process, fuel and oxygen are pressurized and ignited in the combustion chamber and accelerated to supersonic speed through a divergent sonic nozzle, forming a Mach cone. Finally, the particles are sprayed at high speed (>400m/s) and relatively low temperature (<2000℃), with axial powder feeding to provide more uniformly heated particles. HVOF spraying usually does not require subsequent heat treatment, because the low oxidation and the high-velocity particle impact form a dense, firm sprayed coating.
    Plasma transferred arc (PTA): the PTA surfacing process is similar to the tungsten inert gas (TIG) process. The arc is constrained by the nozzle and the shielding gas, producing a constricted columnar arc. The sprayed powders are mainly alloys and carbides, which are fed into the temperature-stable columnar arc through the carrier gas. At the same time, the evenly distributed annular shielding gas can protect the welding area from exposure to air, reducing and preventing oxidation. Among surfacing technologies, PTA has a relatively low dilution rate for the deposited layer on the substrate, maintains the chemical characteristics of the deposited layer and minimizes the penetration depth in the heat-affected zone of the sprayed part
    Nitriding treatment
     
    Hardness of common metal materials for valves:

    Strength
    Strength refers to the ability of a metal material to resist damage (excessive plastic deformation or fracture) under static load. Since loads act in the forms of tension, compression, bending, shear, etc., strength is also divided into tensile strength, compressive strength, bending strength, shear strength, etc. The various strengths are often related to each other; in use, tensile strength is generally taken as the most basic strength indicator.

    Plasticity
    Plasticity refers to the ability of a metal material to undergo plastic deformation (permanent deformation) without damage under load. The commonly used indicators are elongation after fracture and reduction of area.

    Fatigue
    The strength, plasticity and hardness discussed above are all mechanical performance indicators of metals under static load. In fact, many machine parts work under cyclic loads, and under such conditions the parts will fatigue.

    Impact toughness
    A load acting on a machine part at a very high speed is called an impact load, and the ability of a metal to resist damage under an impact load is called impact toughness.

    Corrosion resistance
    Corrosion resistance table of metal materials    Chemical composition of common metal materials    Comparison table of piping and valve materials

CONTACT US

WhatsApp: +8613601902545
Wechat: 13601902545
Phone: +8613601902545
Email: wevalve@outlook.com

Copyright © 2015 www.ourvalve.com