Grades of Metallic Materials



    Forged
    Cast
     
    Forged
    Cast

    ASTM A105

    A182 F316

    A182 F316L

    2.4816/ N06600

    A216 WCB

    A351CF8M

    A361CF3M

    Inconel600 

     

    A182 F11

    A182 F304

    A182 F304L

    ASTM A104

    A217 WC6

    A351CF8

    A351CF3

    WCC

     


Physical Properties of Metallic Materials
    Temperature resistance

     

     

    Temperature range

     

    Working conditions

    Material selection

    Remarks
    Ultra-low temperature
    -254 (liquid hydrogen) to -101 °C (ethylene)
    LNG, air separation Austenitic stainless steels ASTM A351 CF8M, CF3M, CF8 and CF3; ASTM A182 F316, F316L, F304 and F304L; ASTM A433 316, 316L, 304, 304L and CF8D The body material must be an austenitic stainless steel with a face-centred cubic lattice, a copper alloy or an aluminium alloy, and its low-temperature mechanical properties after heat treatment, in particular the low-temperature impact toughness, must meet the requirements of the standard. Deep cryogenic treatment in liquid nitrogen (-196 °C) is required.
    Low temperature
    -100 to -30 °C
    Low-temperature methanol wash

    The low-temperature austenitic stainless steels are ASTM A351 CF8M, CF3M, CF8 and CF3, ASTM A182 F316, F316L, F304 and F304L, and ASTM A433 316, 316L, 304, 304L and CF8D. The ferritic and martensitic steels used for low-temperature pressure parts are ASTM A352 LCA (-32 °C), LCB, LCC (-46 °C), LC1 (-59 °C), LC2, LC211 (-73 °C) and LC3 (-100 °C)

    The initial price of the materials in the ASTM A352 standard is relatively low, but their chemical composition during melting must be covered by a reliable and very strict in-house mill control standard. Their heat-treatment process is complicated and requires repeated quenching and tempering in order to achieve the low-temperature impact toughness required by the standard, so the production cycle is long. When the low-temperature impact toughness fails to meet the standard requirements, the material must not be put into production as low-temperature steel. Therefore, these steels are adopted only where the production batch is large and melting can be done furnace by furnace; under normal circumstances austenitic stainless steel is selected.
    Sub-high temperature
    325 to 425 °C
    Power plant steam, superheated water, atmospheric and vacuum distillation units and delayed coking units of refineries

    For water and steam, WCB, WCC, A105, WC6 and WC9 are mainly used. When the medium is sulphur-bearing oil, C5, CF8, CF3, CF8M and CF3M, which resist sulphide corrosion, are mainly used. These are mostly used in this service; here the CF8, CF8M, CF3 and CF3M valves are not used to resist corrosion by acid solutions but in sulphur-bearing oil and oil-gas pipelines. Under these working conditions the upper limit of the maximum working temperature for CF8, CF8M, CF3 and CF3M is 450 °C

    Carbon steel for valves refers to the WCB and WCC cast steels and the ASTM A105 forged steel of the ASTM A216 standard. The suitable working temperature of carbon steel for valves is -29 to 425 °C. However, for safety and in view of possible fluctuations in the working temperature of the medium, the service temperature of ordinary carbon steel should generally not exceed 400 °C.
    High temperature Class I
    425 to 550 °C
    Power plant superheated steam When the working medium is water or steam, the high-temperature steels WC6 (t ≤ 540 °C) or WC9 (t ≤ 570 °C) can also be used; with sulphur-bearing oil, the high-temperature steel C5 (ZG1Cr5Mo) can also be used The body material of PI class valves is the "high-temperature Class I medium-carbon chromium-nickel rare-earth titanium-bearing high-quality heat-resistant steel" based on CF8 of the ASTM A351 standard
    High temperature Class II
    550 to 650 °C
    Heavy oil catalytic cracking unit The body material of PII class valves is the "high-temperature Class II medium-carbon chromium-nickel rare-earth titanium-tantalum strengthened heat-resistant steel" based on CF8 of the ASTM A351 standard  
    High temperature Class III
    650 to 730 °C
    Heavy oil catalytic cracking unit The "high-temperature Class III medium-carbon chromium-nickel-molybdenum rare-earth titanium-tantalum strengthened heat-resistant steel" based on CF8M of the A351 standard  
    High temperature Class IV
    730 to 816 °C
      The body material of PIV class valves is the "high-temperature Class IV medium-carbon chromium-nickel-molybdenum rare-earth titanium-tantalum strengthened heat-resistant steel" based on CF8M of the ASTM A351 standard. CK-20 and the heat-resistant stainless steels F310 (C content ≥ 0.050%) and F310H of the ASTM A182 standard  
    High temperature Class V
    >816 °C
    Flue gas duct HK-30 and HK-40 high-temperature alloys of the ASTM A297 standard  


    Hardness
    Hardness expresses the ability of a material to resist the indentation of a hard object into its surface. It is one of the important performance indicators of metallic materials. Generally, the higher the hardness, the better the wear resistance. The hardness indicators commonly used are Brinell hardness, Rockwell hardness and Vickers hardness.

    1. Brinell hardness (HB)
    A hardened steel ball of a certain size (generally 10 mm in diameter) is pressed into the surface of the material under a certain load (generally 3000 kg) and held for a period of time; after the load is removed, the ratio of the load to the area of the indentation is the Brinell hardness value (HB), in kgf/mm2 (N/mm2).

    2. Rockwell hardness (HR)
    When HB > 450 or the specimen is too small, Brinell hardness cannot be used and Rockwell hardness is used instead. A diamond cone with a 120° apex angle, or a steel ball of 1.59 or 3.18 mm diameter, is pressed into the surface of the material under a certain load, and the hardness of the material is derived from the depth of the indentation.
    According to the hardness of the material tested, three different scales are used:
    HRA: hardness obtained with a 60 kg load and a diamond cone indenter, used for materials of very high hardness (such as cemented carbide).
    HRB: hardness obtained with a 100 kg load and a hardened steel ball of 1.58 mm diameter, used for materials of lower hardness (such as annealed steel and cast iron).
    HRC: hardness obtained with a 150 kg load and a diamond cone indenter, used for materials of very high hardness (such as hardened steel).
    Stellite hardness 45 HRC, chromium carbide hardness 70 HRC, tungsten carbide hardness 85 HRC

      3. Vickers hardness (HV)
    With a load of up to 120 kg and a diamond square-pyramid indenter with an apex angle of 136° pressed into the surface of the material, the Vickers hardness value HV (kgf/mm2) is the load divided by the surface area of the indentation.

    Hardening methods

    1. Heat treatment, such as surface precipitation hardening heat treatment; the main materials are 440/630;
    2. Stellite hardfacing
    3. Depositing superhard alloys by chemical means, such as hard chromium plating, tungsten carbide and nickel-based alloys; other methods include low-temperature nitriding and ceramic spraying. 304L, 316L and other low-carbon stainless steels are not suitable for Stellite hardfacing.
    According to the German standard DIN 50150, the following is a comparison table of the tensile strength of steel with Vickers hardness, Brinell hardness and Rockwell hardness over commonly used ranges.
    1. Shore hardness (HS) = Brinell hardness (BHN)/10 + 12  2. Shore hardness (HS) = Rockwell hardness (HRC) + 15  3. Brinell hardness (BHN) = Vickers hardness (HV)  4. Rockwell hardness (HRC) = Brinell hardness (BHN)/10 - 3

    High-hardness treatment methods:

    Plasma spraying (APS). The APS process uses a high-voltage arc to heat a gas flow, thereby producing a high-velocity plasma jet. The plasma-forming gas is usually argon containing a small amount of hydrogen or helium, which effectively heats and melts the powder fed into the jet. The temperature at the core of the plasma arc is usually above 10000 K, and the particle impact velocity can reach 250 m/s.
    High-velocity oxygen fuel spraying (HVOF). In HVOF spraying, the fuel and oxygen are pressurised and ignited in a combustion chamber and accelerated to supersonic speed through an expanding sonic nozzle, forming a Mach cone. Finally the particles are sprayed at high velocity (>400 m/s) and relatively low temperature (<2000 °C), with axial powder feed to provide more uniformly heated particles. HVOF spraying usually requires no subsequent heat treatment, because the low oxidation and the high-velocity particle impact produce a dense, firm sprayed coating.
    Plasma transferred arc (PTA) surfacing. The PTA surfacing process is similar to tungsten inert gas (TIG) welding. The arc is constrained by the nozzle and the shielding gas, producing a constricted columnar arc. The spray powders are mainly alloys and carbides, fed through the carrier/plasma gas into the temperature-stable columnar arc. At the same time, a uniformly distributed annular shielding gas protects the welding area from exposure to air, reducing and preventing oxidation. In surfacing technology, PTA gives a relatively low dilution rate of the deposit on the substrate, preserves the chemical characteristics of the deposit and minimises the penetration depth in the heat-affected zone of the sprayed part

    Strength
    Strength refers to the ability of a metallic material to resist failure (excessive plastic deformation or fracture) under static load. Since loads act in tension, compression, bending and shear, strength is correspondingly divided into tensile strength, compressive strength, bending strength and shear strength. The various strengths are often related to one another; in practice, tensile strength is mostly used as the most basic strength indicator.
    Plasticity
    Plasticity refers to the ability of a metallic material to undergo plastic (permanent) deformation without fracture under load. The indicators commonly used are elongation after fracture and reduction of area.

    Fatigue
    The strength, plasticity and hardness discussed above are all mechanical property indicators of metals under static load. In reality, many machine parts work under cyclic loading, and under such conditions the parts will fatigue.
    Impact toughness
    A load applied to a machine part at very high speed is called an impact load, and the ability of a metal to resist failure under an impact load is called impact toughness.
    Corrosion resistance

Corrosion resistance table for metallic materials    Composition table of common metallic materials      Material cross-reference table for pipes and valves Nitriding treatment
Properties of Various Stainless and Alloy Steels
Chromium-molybdenum high-temperature steels
The Cr-Mo high-temperature cast steels selected for valves are mainly WC6, WC9 and C5 (ZG1Cr5Mo) of the ASTM A217 standard, whose corresponding wrought grades are F11, F22 and F5 of ASTM A182 respectively.
(1) Low-chromium grades of Cr-Mo steel
The low-chromium grades of Cr-Mo steel are WC6, WC9, F11 and F22; their suitable working media are water, steam and hydrogen, and they should not be used for sulphur-bearing oil. The suitable working temperature for WC6 and F11 is -29 to 540 °C, and for WC9 and F22 is -29 to 570 °C.
(2) 5% Cr-Mo high-temperature steel
The 5% Cr-Mo high-temperature steels are C5 (ZG1Cr5Mo) and F5; their suitable working media are water, steam, hydrogen and sulphur-bearing oil, etc.
When C5 (ZG1Cr5Mo) is used for water and steam, its maximum working temperature is 600 °C. When used for media such as sulphur-bearing oil, its maximum working temperature is 550 °C. Therefore the working temperature of C5 (ZG1Cr5Mo) is specified as ≤550 °C.

Stainless acid-resistant steels
Stainless acid-resistant steel refers to the chromium-nickel or chromium-nickel-molybdenum stainless acid-resistant steels used in the petrochemical, chemical and fertiliser industries to resist corrosion by nitric acid, sulphuric acid, acetic acid and organic acids. The cast steels are mainly CF8, CF8M, CF3, CF3M, CF8C, CD-4MCu and CN7M of the ASTM A743 or ASTM A744 standard, whose corresponding wrought grades are F304, F316, F304L, F316L, F347 and F53 of the ASTM A182 standard, and UNS N08020 respectively.
(1) Cr-Ni stainless steels
The Cr-Ni stainless acid-resistant steels are CF8, CF3, F304, F304L, CF8C and F347; they are suitable for working media such as nitric acid and other oxidising acids. Their maximum working temperature is ≤200 °C.
(2) Cr-Ni-Mo stainless steels
The Cr-Ni-Mo stainless acid-resistant steels are CF8M, CF3M, F316 and F316L; they are suitable for working media such as acetic acid and other reducing acids.
CF8M and CF3M can replace CF8 and CF3, but CF8 and CF3 cannot replace CF8M and CF3M. Therefore, in the United States and other countries, stainless acid-resistant steel valves mainly use CF8M and CF3M, with a maximum working temperature of ≤200 °C.
(3) CN7M alloy
CN7M alloy has good overall corrosion resistance. It is widely used under severe corrosive conditions, including sulphuric acid, nitric acid, hydrofluoric acid and dilute hydrochloric acid, caustic alkalis, seawater and hot chloride salt solutions; in particular, it can be used in sulphuric acid of various concentrations at temperatures ≤70 °C. The service temperature of CN7M and UNS N08020 alloys is -29 to 450 °C.
(4) Duplex stainless steels
Duplex stainless corrosion-resistant steel (Table 1) is a precipitation-hardening stainless steel containing 35%-40% austenite in a ferrite matrix; its yield strength is about twice that of 19Cr-9Ni austenitic stainless steel, and it has high hardness together with good plasticity and impact toughness. It is particularly suitable for corrosive working conditions that involve both abrasion and erosion, and is therefore widely used in strongly oxidising and reducing acid services, and has special resistance to stress corrosion cracking in chloride-containing environments. The service temperature of CD-4MCu, CD3MN, CE3MN and F53 duplex stainless steels is -29 to 316 °C.

Corrosion-resistant nickel-based alloys
Corrosion-resistant nickel-based alloy valves mainly use the cast Monel alloy (M35-1), cast nickel alloy (CZ-100), Inconel alloy (CY-40), Hastelloy B (N-12MV, N-7M) and Hastelloy C (CW-12MW, CW-7M, CW-6MC, CW-2M) of the ASTM A494 standard.
The Monel wrought materials used for corrosion-resistant Monel alloy valves are mainly UNS N04400 (Monel 400) and UNS N05500 (Monel K500). Cast nickel alloy has no corresponding wrought material; the wrought materials of Inconel alloy are Inconel 600 and Inconel 625, etc.
(1) Monel alloy
Monel alloy has relatively high strength and toughness, and in particular excellent resistance to corrosion by reducing acids, strong alkaline media and seawater. It is therefore usually used to manufacture equipment and valves for conveying hydrofluoric acid, brine, neutral media, alkaline salts and reducing acids, and is also suitable for dry chlorine gas, hydrogen chloride gas, high-temperature chlorine gas at 425 °C and high-temperature hydrogen chloride gas at 450 °C, but it does not resist corrosion by sulphur-bearing media and oxidising media (such as nitric acid and media with a high oxygen content). The material code for valves made entirely of Monel alloy is MM; for valves with Monel alloy trim, the code is C/M when the body is carbon steel, P/M when the body is CF8 and R/M when the body is CF8M. The suitable working temperature of Monel M35-1, Monel 400 and Monel K500 alloys is -29 to 480 °C.
(2) Cast nickel alloy
The chemical composition of cast nickel alloy (CZ-100) is 95% Ni and 1.00% C, and it has no corresponding wrought material. When CZ-100 is used in high-temperature, high-concentration or anhydrous alkali solutions, it has excellent corrosion resistance. CZ-100 is often used in chlor-alkali production with highly corrosive concentrations (including molten anhydrous caustic soda) and in applications where the product must not be contaminated by metals such as copper and iron. The material code for cast nickel alloy CZ-100 valves is Ni. The suitable working temperature of CZ-100 alloy is -29 to 316 °C.
(3) Inconel alloy
Inconel alloy CY-40 and Inconel 600 (ASTMB564 N06600), etc. are mainly used to resist stress corrosion, and are especially suitable for high-concentration chloride media; when the Ni content is ≥45%, it has an "immune" effect against chloride stress corrosion. In addition, it resists corrosion by boiling concentrated nitric acid, fuming nitric acid, and high-temperature gases and combustion products containing sulphur and vanadium.
Inconel alloys have been widely used to manufacture components of boiler feedwater systems in nuclear power plants, because they are safer than stainless steel. At the same time, they are also suitable for industrial production requiring high strength, high-pressure sealing and high corrosion resistance, as well as resistance to mechanical wear and oxidation at high temperature. For example, large fertiliser plants use Inconel 600 or Inconel 625 alloy (the wrought grade of Hastelloy CW-6MC) to manufacture high-pressure (600-1500 LB) high-concentration oxygen valves. The material code for CY-40 and Inconel 600 alloy valves is In. The suitable working temperature is -29 to 650 °C.
(4) Hastelloy
Hastelloy is a commercial name covering a series of alloy grades; those used for corrosion-resistant valves are mainly the two families Hastelloy B and Hastelloy C.
The cast alloy grades of Hastelloy B in the ASTM A494 standard are N-12MV (N-12M-1) and N-7M (called N-12M-2 in some literature and also known as Chlorimet 2 alloy), and its wrought grade is UNS N10665 in the ASTM B335 standard. Hastelloy B resists corrosion by hydrochloric acid of all concentrations and also resists non-oxidising salts and acids. For Hastelloy B corrosion-resistant valves, from the standpoint of corrosion resistance and resistance to intergranular corrosion, the low-carbon grade Hastelloy B (N-7M) should be selected. The valve industry has not yet specified a material code for Hastelloy; the material code of Hastelloy B valves can be expressed directly by their cast alloy grade. The suitable working temperature of Hastelloy B is -29 to 425 °C.
The cast alloy grades of Hastelloy C are CW-12MW (called CW-12M-1 in some literature) and CW-7M (CW-12M-2, also known as Chlorimet 3 alloy), and Hastelloy C-276 alloy, whose cast alloy grade is CW-6MC, and Hastelloy C-4 alloy, whose cast alloy grade is CW-2M. The corresponding wrought grades of the cast Hastelloy alloys CW-7M, CW-12MW, CW-6MC and CW-2M are UNS N10001, UNS N10003, UNS N10276 and UNS N06455 respectively. Hastelloy C resists corrosion by oxidising solvents, and by low-concentration hydrochloric acid and nitric acid at room temperature.
The first generation Hastelloy C (0Cr16Ni60Mo16W4) is characterised by excellent corrosion resistance in strongly corrosive oxidising and reducing acid media, but because high-nickel corrosion-resistant alloys have an austenitic structure and because Ni reduces the solid solubility of C in austenite, both the Ni-Mo Hastelloy B and the Ni-Mo-Cr Hastelloy C alloys have a fairly serious tendency to, or sensitivity to, intergranular corrosion, and at high temperature can also suffer stress corrosion and crevice corrosion. In order to overcome intergranular corrosion, the second-generation Hastelloy C-276 (C reduced from 0.03% to 0.02%) and the third-generation Hastelloy C-4 were introduced; these are characterised by low Si (Si ≤0.08%) and ultra-low C (C ≤0.015%), with reduced Fe and W contents and the addition of the stabilising alloying element Ti, etc.
For Hastelloy C corrosion-resistant valves, from the standpoint of corrosion resistance and resistance to intergranular corrosion, Hastelloy C-276 (CW-6MC) and Hastelloy C-4 (CW-2M) should be selected. Hastelloy C valves have many material codes and differ greatly in performance and working temperature, so CW-12MW, CW-7M, CW-6MC and CW-2M are designated HC-12, HC-7, HC-276 and HC-4 respectively, or expressed directly by their cast alloy grades.
The suitable working temperature of Hastelloy CW-7M and UNS N10001 alloy is -29 to 425 °C, of Hastelloy CW-12MW and UNS N10003 alloy is -29 to 700 °C, of Hastelloy CW-6MC and UNS N10276 alloy is -29 to 676 °C, and of Hastelloy CW-2M and UNS N06455 alloy is -29 to 425 °C.

Titanium alloys
Titanium (Ti) offers high strength, low weight, sufficiently high heat resistance and low-temperature toughness, and good machinability and weldability. In valve production, cast commercially pure titanium and wrought commercially pure titanium ZTA2 are mainly used.
Titanium's behaviour towards corrosive media - corrosion resistance, lack of corrosion resistance, or even ignition and explosion - varies with temperature and other working conditions. Therefore, when ordering and selecting for design, the nature of the service medium (concentration, temperature, etc.) must be clearly specified.
Titanium valves have excellent corrosion resistance in many strongly oxidising corrosive media and in neutral media.
Titanium has excellent corrosion resistance in nitric acid below the boiling point at concentrations ≤80%. In fuming nitric acid, however, when the NO2 content exceeds 2% and the water content is insufficient, titanium reacts with the fuming nitric acid and an explosion may occur; therefore titanium is generally not used for high-temperature nitric acid above 80% concentration.
Titanium is not resistant to sulphuric acid, and has moderate corrosion resistance in hydrochloric acid. It is generally considered that commercially pure titanium can be used in hydrochloric acid at 7.5% concentration at room temperature, 3% at 60 °C and 0.5% at 100 °C; titanium can also be used in phosphoric acid at 30% concentration at 35 °C, 10% at 60 °C and 3% at 100 °C.
Titanium is not resistant to HF (hydrofluoric acid) and is also not resistant to acidic fluoride solutions; titanium is resistant to boric acid and chromic acid, and can be used in hydroiodic acid and hydrobromic acid.
Titanium can be used in a mixed acid of 10% sulphuric acid and 90% nitric acid at 60 °C, in a mixed acid of boiling 1% hydrochloric acid and 5% nitric acid, and in aqua regia at room temperature (note: aqua regia is a mixture of 3 volumes of concentrated hydrochloric acid and 1 volume of concentrated nitric acid).
At room temperature titanium is completely resistant to barium hydroxide, calcium hydroxide, magnesium hydroxide, sodium hydroxide and potassium hydroxide solutions of all concentrations, but it must not be used in boiling sodium hydroxide and potassium hydroxide. Ammonia contained in the alkali will aggravate the corrosion of titanium.
The maximum working temperature of titanium in tap water, river water and air is 300 °C. Titanium can be used in seawater at velocities up to 20 m/s; titanium has very high corrosion resistance in seawater at temperatures ≤120 °C, but if the temperature is above 120 °C, pitting corrosion and crevice corrosion may occur.
Apart from formic acid, oxalic acid and fairly concentrated citric acid (concentration ≥50%), titanium has excellent corrosion resistance to all organic acids; however, when the water content of the organic acid is too low (<0.1%), titanium is prone to pitting corrosion.
Titanium has excellent corrosion resistance in hydrocarbons and chlorinated hydrocarbons. In dry chlorine gas titanium reacts violently to form TiCl4, with a risk of ignition, but in wet chlorine (water content 0.3%-1.5%) titanium has very good corrosion resistance.
Titanium is stable in dry HCl at 20-160 °C, but in wet hydrogen chloride the hydrochloric acid causes corrosion of titanium.
The pitting potential of titanium in chloride solutions is higher than that of stainless steel, and titanium has better resistance to chloride pitting than stainless steel, so titanium is widely used in chloride solutions.
At temperatures ≤80 °C titanium generally does not pit, but in high-temperature chloride solutions of medium concentration (such as 25% aluminium chloride solution at 100 °C, 70% calcium chloride solution at 175 °C, 25% magnesium chloride solution at 200 °C and 75% zinc chloride solution at 200 °C) pitting corrosion occurs fairly easily.
Effect of Various Chemical Elements on the Properties of Metallic Materials
    C: The higher the carbon content, the higher the hardness of the steel and the better the wear resistance, but the poorer the plasticity and toughness. As the carbon content in steel increases, the yield point and tensile strength rise, but plasticity and impact resistance decrease; when the carbon content exceeds 0.23%, the weldability of the steel deteriorates, so low-alloy structural steels used for welding generally contain no more than 0.20% carbon. A high carbon content also reduces the resistance of steel to atmospheric corrosion - high-carbon steel stored in open yards rusts easily. In addition, carbon increases the cold brittleness and strain-ageing sensitivity of steel.

    S: Sulphur is a harmful impurity in steel. Steel with a high sulphur content is liable to brittle cracking when hot forming under pressure, a phenomenon usually called hot shortness. Sulphur is also a harmful element under normal conditions. It causes hot shortness in steel, reduces the ductility and toughness of the steel and causes cracks during forging and rolling. Sulphur is also unfavourable to weldability and reduces corrosion resistance. Therefore the sulphur content is usually required to be less than 0.055%, and high-quality steel requires less than 0.040%. Adding 0.08-0.20% sulphur to steel can improve machinability; this steel is usually called free-cutting steel.

    P: Phosphorus can markedly reduce the plasticity and toughness of steel, and the effect is even more serious at low temperature; this phenomenon is called cold brittleness. In high-quality steel the sulphur and phosphorus contents should be strictly controlled. On the other hand, when low-carbon steel contains relatively high sulphur and phosphorus, the chips break easily during cutting, which is favourable for improving the machinability of the steel. Under normal circumstances phosphorus is a harmful element in steel: it increases the cold brittleness of steel, worsens weldability, reduces plasticity and deteriorates cold-bending performance. Therefore the phosphorus content in steel is usually required to be less than 0.045%, and even lower for high-quality steel.

    Mn: Manganese can increase the strength of steel, eliminate or weaken the adverse effects of sulphur, and improve the hardenability of steel. High-alloy steel with a very high manganese content (high-manganese steel) has good wear resistance and other physical properties. In the steelmaking process manganese is a good deoxidiser and desulphuriser, and ordinary steel contains 0.30-0.50% manganese. When more than 0.70% is added to carbon steel it is regarded as "manganese steel"; such steel not only has sufficient toughness but also higher strength and hardness, improves the hardenability and improves the hot-working performance of the steel - for example, 16Mn steel has a yield point 40% higher than A3. Steel containing 11-14% manganese has extremely high wear resistance and is used for excavator buckets, ball-mill liners, etc. Increasing the manganese content weakens the corrosion resistance of steel and lowers weldability.

    Si: An increase in the silicon content can increase the hardness of steel, but plasticity and toughness decrease. A certain amount of silicon in electrical steels can improve the soft magnetic properties. In the steelmaking process silicon is added as a reducing agent and deoxidiser, so killed steel contains 0.15-0.30% silicon. If the silicon content in steel exceeds 0.50-0.60%, silicon counts as an alloying element. Silicon can markedly raise the elastic limit, yield point and tensile strength of steel, and is therefore widely used in spring steels. Adding 1.0-1.2% silicon to quenched and tempered structural steel can increase strength by 15-20%. Combined with molybdenum, tungsten, chromium, etc., silicon has the effect of improving corrosion resistance and oxidation resistance, and can be used to make heat-resistant steel. Low-carbon steel containing 1-4% silicon has extremely high magnetic permeability and is used in the electrical industry to make silicon steel sheets. An increase in the silicon content reduces the weldability of steel.

    W: Tungsten can improve the red hardness and hot strength of steel and can also improve the wear resistance of steel. Tungsten has a high melting point and high density and is an expensive alloying element. Tungsten forms tungsten carbide with carbon, which has very high hardness and wear resistance. Adding tungsten to tool steel can markedly improve the red hardness and hot strength, for use in cutting tools and forging dies.

    Cr: Chromium can improve the hardenability and wear resistance of steel, improve the oxidation resistance of steel and increase the corrosion resistance of steel. In structural and tool steels, chromium can markedly increase strength, hardness and wear resistance, but at the same time reduce plasticity and toughness. Chromium can also improve the oxidation resistance and corrosion resistance of steel, and is therefore an important alloying element of stainless and heat-resistant steels.

    V: Vanadium can refine the grain structure of steel and improve the strength, toughness and wear resistance of steel. When it dissolves in austenite at high temperature it can increase the hardenability of steel; conversely, when it exists in the form of carbides it reduces the hardenability of steel. Vanadium is an excellent deoxidiser for steel. Adding 0.5% vanadium to steel can refine the grain structure and improve strength and toughness. The carbides formed by vanadium and carbon can improve resistance to hydrogen corrosion at high temperature and high pressure.

    Mo: Molybdenum can markedly improve the hardenability of steel, improve hot strength, prevent temper brittleness, and increase residual magnetism and coercivity. Molybdenum can refine the grains of steel and maintain sufficient strength and creep resistance at high temperature (long-term deformation under stress at high temperature is called creep). Adding molybdenum to structural steel can improve the mechanical properties. It can also suppress the brittleness of alloy steel caused by fire. In tool steel it can improve red hardness.

    Ti: Titanium can refine the grain structure of steel, thereby improving the strength and toughness of steel. In stainless steel, titanium can eliminate or alleviate intergranular corrosion of the steel. Titanium is a strong deoxidiser in steel. It can make the internal structure of steel dense and refine the grains; reduce strain-ageing sensitivity and cold brittleness; and improve weldability. Adding an appropriate amount of titanium to 18Cr-9Ni austenitic stainless steel can avoid intergranular corrosion.

    Ni: Nickel can improve the strength and toughness of steel and improve hardenability; at high contents it can markedly change some physical properties of steel and alloys and improve the corrosion resistance of steel. Nickel can increase the strength of steel while maintaining good plasticity and toughness. Nickel has relatively high resistance to corrosion by acids and alkalis, and has rust resistance and heat resistance at high temperature. However, since nickel is a relatively scarce resource, other alloying elements should be used as far as possible to replace nickel-chromium steel.

    B: The effect of boron is that when steel contains a trace amount (0.001-0.005%) of boron, the hardenability of the steel can be increased several times over.

    AI: Aluminium can refine the grain structure of steel, inhibit the strain ageing of low-carbon steel and improve the toughness of steel at low temperature. Aluminium can also improve the oxidation resistance of steel and the wear resistance and fatigue strength of nitrided steel. Aluminium is a commonly used deoxidiser in steel. Adding a small amount of aluminium to steel can refine the grains and improve impact toughness, as in 08Al steel used for deep-drawn sheet. Aluminium also has oxidation resistance and corrosion resistance; when aluminium is used together with chromium and silicon, it can markedly improve the resistance of steel to scaling at high temperature and to high-temperature corrosion. The disadvantage of aluminium is that it affects the hot-working performance, welding performance and machining performance of steel.

    Cu: The outstanding effect of copper in steel is to improve the atmospheric corrosion resistance of ordinary low-alloy steel; especially when used together with P, it can increase the strength and the yield ratio of steel. Copper at 2-3% in austenitic stainless steel can improve the resistance to corrosion by sulphuric acid, hydrochloric acid and phosphoric acid, and the stability of resistance to stress corrosion.

Copyright © 2015 www.ourvalve.com